One, rotten edge: 1, mesh edge mesh wire broken rotten: timely sorting network edge, clear mesh wire, prevent mesh edge points. 2, mesh edge slurry: change
Good surface pulp, core pulp baffle plate, increase the edge water force. 3. Poor use of water needle: make good use of edge spray water or increase the water spraying intensity.
Check the working status of water needle at any time, the main filter well, choose the linear fine water needle. 4. Gluing edge: replace in time
Cloth strips are placed on both sides of the sizing machine to prevent the leakage of rubber onto the water-cooling roller. During the paper breaking, clean the rubber on the water-cooling roller and press it
Spray device can be added at both ends of the roller on the optical machine to prevent rubber from sticking to the edge of the roller. 5, net deviation: at any time to clean the guide roll slurry, indeed
Keep the running tension of forming net and dry net consistent, ensure the guide roller and true empty box are not shifted, and each roller runs smoothly